Injection Molding Cycle Time Calculator
Cycle time is the most casually guessed number in a molding quote — 20 seconds or 35 seconds doubles the machine cost per part. This tool solves one-dimensional cooling, then adds open-close and injection hold to give the cycle and hourly output.
| Cooling time | — s |
| Cooling share of cycle | — % |
| Output | — parts/hour |
| Cooling added at +10% wall | — s |
Range ±30%. The one-dimensional slab model assumes heat flows only through the wall and ignores ribs, inserts, the gate region and actual cooling-circuit performance. It tells you the order of magnitude a quote should sit in — the real cycle comes from a trial run.
The formula and where it comes from
Cooling time follows the classic transient-conduction solution for a flat slab:
t_cool = s² / (π²·α) · ln( 4/π · (T_melt − T_mold) / (T_eject − T_mold) )
t_cycle = t_cool + open/close + injection hold
parts/h = 3600 ÷ t_cycle × cavities The critical term is s²: double the wall and cooling roughly quadruples. That is why taking a 3 mm wall down to 2 mm halves the cycle, and why wall-thickness reduction remains the first lever in molding cost work.
Worked example
2 mm ABS (α = 0.09), melt 230 °C, mold 50 °C, eject 90 °C, 3 s open-close, 2 s injection, one cavity:
| Cooling time | 7.86 s |
| Cycle (7.86 + 3 + 2) | 12.86 s |
| Shots / parts per hour | 280 / 280 |
| Cooling share | 61% |
| Wall at 2.2 mm (+10%) | +1.65 s cooling, +13% cycle |
Push the wall to 3 mm and cooling becomes 17.7 s, the cycle 22.7 s, output 159 parts/hour: the same machine delivers 43% fewer parts, so machine cost per part rises 76%.
How cycle time enters cost
Machine cost = hourly rate ÷ parts per hour. At 60 CNY/hour and 280 parts/hour, that is 0.21 CNY per part; at a 22-second cycle it is 0.38 CNY. Feed the cycle into the molding cost calculator together with material and tooling amortisation to get a complete should-cost.
Four variables that move the cycle
- Wall thickness — squared relationship, the most sensitive lever. Keep ribs at 60% of the main wall or they will not freeze with it.
- Ejection temperature — eject earlier and the cycle shortens, but too early causes whitening and warpage. Thin-wall parts commonly eject at 80–100 °C.
- Mold temperature — hotter molds improve flow and appearance, but reduce the driving temperature difference to ejection, so cooling can slow down.
- Open-close and part removal — robots, slides and lifters extend this segment; multi-cavity tools dilute it.
Not included
- Physics-based hold time (set by gate freeze and requiring mold-flow analysis)
- Cooling-circuit design and its real heat-transfer capability
- Mechanical time for slides, lifters and two-stage ejection
- Mold changes, purging and trial runs
- Die casting and blow molding cycles — same equation shape, different α and temperatures
FAQ
Why maximum wall instead of average?
Because a part cannot eject until its slowest region freezes. Average wall thickness smears the wait in thick sections and yields an optimistic cycle. With uneven geometry, calculate the thickest section — then consider a design change that thins it.
Shouldn't a hotter mold cool faster?
Not necessarily. Cooling is driven by the difference between melt and mold. Raising mold temperature shrinks that difference, though a higher ejection temperature (softer parts can be ejected) can more than compensate. In production, mold temperature is set by appearance and warpage, not by cycle optimisation.
Do cavities scale output linearly?
In theory yes; in practice clamping force, runner balance and part removal take a cut. Four-cavity tools often run 10–20% longer cycles than single-cavity because open-close strokes and removal are more complex. This tool assumes linear scaling, which is the optimistic case.