Blow Molding Cost Calculator
Bottles, jerry cans, shampoo packs, air ducts, hollow cases — anything blown into a cavity is extrusion blow molding. The unit there is not a metre of profile or a moulding shot; it is one parison: a tube of melt drops from the die head, the mould closes on it, air inflates it, it cools, the mould opens, the flash is trimmed. This tool splits the part cost into material, machine time, mould amortisation and trimming, and answers a question that is usually glossed over: how much does regrinding the flash actually save?
1. Inputs
| Material (net of regrind credit, scaled by yield) | — CNY |
| Machine time | — CNY |
| Mould amortisation | — CNY |
| Trimming / deflashing | — CNY |
| Material before credit | — CNY |
| Regrind credit | — CNY |
| Parison weight per part | — g |
| Net material weight (regrind at 50%) | — g |
| Flash / trim weight | — g |
| Cycle time per part | — s |
| Good output | — parts/h |
±30%. Material and cycle time are the reliable inputs; two others drift most: the flash ratio (up to 40% on large parts, just over 10% on narrow-neck bottles) and the trimming rate (0.1 CNY hand-trimmed, 0.3 CNY and up with an automatic deflasher). This is not a supplier quote — it says what the resin and machine time should cost.
Formula
yield = 1 − scrap rate
gross material = parison_g ÷ 1000 × price ÷ yield
net material (g) = parison_g × (1 − regrind ratio × 0.5)
material = net_g ÷ 1000 × price ÷ yield
regrind credit = gross material − material
cycle per part = cycle per shot ÷ cavities
machine = cycle per part ÷ 3600 × rate ÷ yield
mould amort. = mould cost ÷ cavities ÷ mould life (shots)
trimming = trim rate per part
total = material + machine + mould + trimming Material and machine time are both divided by yield: a scrapped part burns resin and occupies that slice of machine time. Mould amortisation and trimming are per-part fixed items and do not move with scrap — the mould cost is consumed per shot regardless. Regrind is credited at 50% of virgin price, the one parameter here that is not straight book arithmetic; the reason is in the section below.
What the inputs mean
- Parison weight — the melt tube as it leaves the die head, including neck allowance, bottom allowance and whatever becomes flash. Without a scale, use bottle weight × 1.2–1.4: small bottles waste proportionally more, large drums less.
- Cycle per shot — close, blow, cool, open, eject. Thick-wall large parts run 60 s and above; thin-wall small bottles do 12–18 s.
- Cavities — doubling cavities halves cycle time per part and halves mould amortisation, while mould cost itself usually does not double (platens and cooling circuits are shared). More cavities almost always helps.
- Machine rate — extruder, clamp, blow system and chiller: depreciation, power, operator. Small machines 120–180 CNY/h; large ones with a accumulator head 240–400 CNY/h.
- Mould cost and life — aluminium is cheap but lasts tens of thousands of shots; steel costs more and reaches a million. Amortisation is mould cost ÷ cavities ÷ life, so a wrong life figure doubles or halves the part price.
- Trimming — every blown part has flash: the ring at the parting line and the pinch-off tab. Hand trimming is cheap, an automatic deflasher costs more but is consistent.
- Regrind ratio — flash and trim as a share of parison weight. It can be ground back in, so it is not a total loss, but it is not virgin resin either.
Worked examples
HDPE, 120 g parison, 2 cavities, 25 s cycle, 180 CNY/h, 60,000 CNY mould over 1,000,000 shots, 0.12 CNY trimming, 20% regrind, 4% scrap (page defaults):
| Yield | 1 − 0.04 = 0.96 |
| Gross material | 120 ÷ 1000 × 9.50 = 1.14 → ÷0.96 = 1.19 CNY |
| Net material weight | 120 × (1 − 0.20 × 0.5) = 108 g |
| Material | 108 ÷ 1000 × 9.50 = 1.026 → ÷0.96 = 1.07 CNY (credit 0.12) |
| Cycle per part | 25 ÷ 2 = 12.5 s |
| Machine | 12.5 ÷ 3600 × 180 = 0.625 → ÷0.96 = 0.65 CNY |
| Mould amortisation | 60,000 ÷ 2 ÷ 1,000,000 = 0.03 CNY |
| Trimming | 0.12 CNY |
| Total | 1.07 + 0.65 + 0.03 + 0.12 = ¥1.87 per part, 276.5 parts/h |
The same model with other conditions:
| One cavity, 30 s cycle, 30,000 CNY mould, 10% regrind, 2% scrap | material 1.11 + machine 1.53 + mould 0.03 + trim 0.12 = ¥2.79 |
| 5 L drum: 500 g parison, one cavity, 60 s cycle, 240 CNY/h, 120,000 CNY mould over 500,000 shots, 0.30 trimming | material 4.50 + machine 4.21 + mould 0.24 + trim 0.30 = ¥9.25 |
| Same drum, mould life cut to 50,000 shots (aluminium, trial batch) | mould 0.24 → 2.40, total ¥11.41 |
The third row is the cost that gets missed: the same drum costs 0.24 CNY of mould per part over 500,000 shots of steel tooling and 2.40 CNY over 50,000 shots of aluminium — more than the machine time. A high quote on a pilot batch usually means the mould has not been paid off yet, not that the moulder is gouging.
Why the parison is heavier than the part
The parison is a straight tube; the part is that tube inflated into the cavity. The difference goes to three places: the parting-line flash (a full ring), the pinch-off tab at the base or neck, and the wall allowance that keeps the blow-out even. Parison weight is therefore 1.2–1.4× the finished weight — higher for large or square parts, lower for narrow-neck round bottles. This is why a blow molding cost sheet has to start from the parison: backing material cost out of finished weight understates it by 20–40%.
Why regrind is credited at 50%
Ground flash can go back in, but the market price for regrind is never the virgin price: the polymer has been through a second heat history, impact strength drops, colour darkens (useless for clear bottles), and above roughly 30% regrind the wall thickness starts to scatter. Add the grinder's power and labour and the real credit lands at 40–60% of virgin price. This tool uses 50% as a conservative ceiling: if your regrind is really worth 30%, material cost is higher, not lower.
Blow molding vs injection molding vs extrusion
| Shape | Hollow, thin-walled, single opening (bottle, drum, case) → blow molding; solid or with complex internal features → injection molding |
| Volume | Blow moulds are an order of magnitude cheaper than injection moulds — a few thousand parts can justify one; injection needs tens of thousands |
| Tolerance | Wall thickness ±15% from the start; if a mating face needs ±0.1 mm, blow molding cannot hold it |
| Cost structure | Material 55–70%, machine 20–35%, mould usually under 5% — unless the life figure is too short |
For constant-section long products (pipe, profile, sheet) use the extrusion cost calculator; for the die head investment behind the parison, use the extrusion die cost estimator.
Four common mistakes
- Using finished weight as parison weight — understates resin by 20–40%, the single most common systematic error in these quotes.
- Forgetting trimming — no blown part skips it: 0.05–0.15 CNY on small parts, 0.3 CNY and up with automatic deflashing on large ones.
- Treating the mould as a one-off with an invented life — a tenfold life error is a tenfold amortisation error. Aluminium tooling entered as a million shots looks great and needs replacing within a month.
- Crediting regrind at 100% — flash is not money, the discounted regrind value is. Crediting it in full turns a cost sheet into a profit sheet.
Not included
- Resin drying energy (PET, PC and PA must be dried 4–8 h before blowing)
- Caps, labels, printing, sleeving and inner liners
- Packaging, freight, tax, margin and factory overhead
- Mould changes and start-up scrap (negligible in continuous runs, significant in pilot batches)
- Multi-layer co-extrusion heads and their distributors
FAQ
Why does doubling cavities not halve the part cost?
Only machine time and mould amortisation scale with cavities; material and trimming are per part. In the default example, going from 2 cavities to 1 pushes machine cost from 0.65 to 1.30 and mould from 0.03 to 0.06, while material (1.07) and trimming (0.12) stay put — the total moves from 1.87 to 2.79, up 49%, not double.
Should mould changes and start-up be in the cycle time?
Not in continuous runs: one change covers hundreds of thousands of parts and rounds to nothing. In a pilot batch of a few thousand, it matters — two hours of changeover and tens of kilos of start-up scrap can be 20–30% of the part price. Spread them over the batch size or quote the batch as a whole.
The estimate is far below the moulder's quote — what am I missing?
Check three things first: whether mould cost is inside the part price (some shops invoice it separately), whether trimming is automated, and whether drying and inner liners are included. Then the exclusions — bottles are bulky, so freight often costs more than the conversion. A 20% gap is normal; a twofold gap means asking about mould life and the actual resin grade (regrind-filled compounds are common).