CostKit

Plastic Material Selector

Every injection moulding cost page has a resin dropdown, but the question that comes first is different: which resin can this part actually use? This tool works the other way round — you give the hard requirements (budget, service temperature, food contact, transparency, impact, outdoor use), anything that fails is excluded with a stated reason, and the rest are scored on "cheap and sufficient". Everything runs locally in the browser; no drawings or parameters are uploaded.

1. Inputs

Delivered price for standard moulding grade bought by the tonne. Above this the resin is excluded outright.
The part's real working temperature plus a margin — not the melting point. Indoor parts 40–60 °C, hot-water parts 90 °C, under-bonnet 120 °C.

—

—

ResinVerdict
ABS—
Polypropylene (PP)—
Polyethylene (PE)—
Polystyrene (PS)—
Polycarbonate (PC)—
Nylon 66 (PA66)—
Acetal (POM)—
Acrylic (PMMA)—

Once you have a first pick, carry it into the resin dropdown of the injection moulding cost or part weight and material calculator. The four flags answer "can this resin be used at all", not "is it good enough" — wall thickness, ribs and assembly stress need mould-flow analysis and trial shots.

This is a shortlist, not a material decision. Eight resins cover the commodity grades plus the common engineering grades. A real selection also has to clear flame rating, chemical resistance, long-term ageing, supplier grade and minimum order quantity. The point of this tool is to cross out the obviously unusable options so you approach suppliers with two or three candidates instead of guessing among a dozen grades.

Scoring rules

Step 1  Hard requirements (fail = excluded, first reason wins, checked in this order)
  1. price > ceiling                     -> "above budget"
  2. max service temp < min temp needed  -> "too low a service temperature"
  3. food contact needed, not food grade -> "not food-contact grade"
  4. transparency needed, opaque resin   -> "not transparent"
  5. impact needed, brittle resin        -> "brittle, no impact resistance"
  6. outdoor needed, not UV rated        -> "not UV/outdoor rated"

Step 2  Score (passing resins only)
  budget headroom  = round(40 × (ceiling − price) ÷ ceiling)     0–40, cheaper scores higher
  temperature margin = max service temp − min temp needed
                     ≥30 °C -> 20 pts ; ≥15 °C -> 12 pts ; ≥0 °C -> 6 pts
  total = budget headroom + temperature margin                   6–60

Step 3  Rank: highest score wins; ties go to the cheaper resin

Two rules deserve a note. Hard requirements are not scored: using a non-food-grade resin in a food-contact part is not "a few points worse", it is simply not allowed, and a low score still gets picked out of a long list. More than 30 °C of temperature margin adds nothing: moulding an ambient-temperature housing in 150 °C PA66 is not better, only more expensive. The margin score only moves between "just enough / comfortable / abundant", which stops the tool from always recommending the most heat-resistant resin on the shelf.

Built-in resin property table

The price column is shared with the injection moulding cost page — one edit changes both.

ResinPrice (CNY/kg)Continuous service temp (°C) Food contactTransparentImpactOutdoor
ABS ABS 13.00 80 no no yes no
PP Polypropylene 10.00 100 yes no yes no
PE Polyethylene 9.00 80 yes no yes yes
PS Polystyrene 11.00 70 yes yes no no
PC Polycarbonate 22.00 120 yes yes yes yes
PA66 Nylon 66 26.00 150 yes no yes yes
POM Acetal (POM) 18.00 100 yes no yes yes
PMMA Acrylic (PMMA) 17.00 80 no yes no yes

Prices are public market references for standard moulding grades bought by the tonne; flame-retardant, glass-filled, medical and clarified grades cost noticeably more. The temperature is the continuous service ceiling, not the heat deflection temperature (HDT) and not a short-term peak — peaks typically run 20–40 °C higher. Always confirm against the supplier datasheet.

Worked examples

Page defaults: 20 CNY/kg ceiling, 70 °C minimum, food contact and impact required, no transparency or outdoor requirement.

ABS1300 ≤ 2000; 80 ≥ 70; but not food grade → excluded
PPpasses: round(40 × (2000 − 1000) ÷ 2000) = 20; margin 100 − 70 = 30 → 20 pts → 40 pts
PEpasses: round(40 × 1100 ÷ 2000) = 22; margin 10 → 6 pts → 28 pts
PS70 ≥ 70 but brittle → excluded
PC / PA662200 / 2600 > 2000 → excluded (over budget)
POMpasses: round(40 × 200 ÷ 2000) = 4; margin 30 → 20 pts → 24 pts
PMMAnot food grade → excluded
Result3 pass, first pick PP (40 pts), backups PE (28) and POM (24)

Change the conditions to a few real scenarios and the answer moves a lot:

Outdoor 5 L chemical drum: 15 CNY/kg, 60 °C, impact + outdoor ABS and PP fail on weatherability, PC / PA66 / POM / PMMA are all over budget, leaving PE: round(40 × 600 ÷ 1500) = 16 + 12 (margin 20) = 28 pts
Transparent lamp cover: 30 CNY/kg, 90 °C, transparent ABS / PE / PS / PMMA are too low on temperature, PP / PA66 / POM are opaque, leaving PC: round(40 × 800 ÷ 3000) = 11 + 20 = 31 pts
Ceiling exactly 10 CNY/kg, 100 °C required PP lands exactly on the ceiling (≤ passes): 0 + 0 margin → 6 pts, and it is the only survivor; PE tops out at 80 °C and is excluded

The second row is worth pausing on: "transparent + 90 °C" leaves PC as the only option out of eight. That is not the tool being lazy, that is the reality of the shelf — transparent PS and PMMA stop at 70–80 °C, and the heat-resistant PP, PA66 and POM are all opaque. Either relax the temperature (go PMMA) or accept PC's price (22 CNY/kg, more than double PP).

Four common mistakes

Not covered

After picking a resin, carry on with the injection moulding cost, part weight and material, cycle time and clamp force and tonnage calculators; if the process route is still open, start from the process selection guide.

FAQ

Why no PET, PBT, TPU or PPS?

The table is shared with the injection moulding cost page and keeps only the eight most common resins: four commodity grades (PP / PE / PS / ABS) plus four engineering grades (PC / PA66 / POM / PMMA). PET mostly goes to bottle-grade blow moulding, TPU to elastomer parts and PPS is a specialty engineering resin — mixing them in would distort the scoring. For those, enter their price and temperature as a custom material in the injection moulding cost calculator.

Why does a tie go to the cheaper resin instead of the better performer?

Because "good enough" is already baked into the score: everything that gets scored passed all your hard requirements. At equal qualification, the extra money buys headroom you do not need. If a property is genuinely required, make it a hard requirement (tick impact, for example) and the tool will exclude resins that fail it rather than hinting at it through the score.

What if nothing passes?

Look at the distribution of reasons: if most say "above budget", raise the ceiling; if most say "too low a service temperature", put the temperature back to the real working value. If the reasons split evenly, the requirements themselves conflict — "transparent + 120 °C + 10 CNY/kg" does not exist among the eight commodity resins, so change the approach (glass, a heat-resistant coating, or a higher budget).

References

  1. Plastics — Methods for determining the density of non-cellular plastics ISO · ISO 1183
  2. Plastics raw material pricing Sci99 · 公开行情

Basis for the parameters above. Links go to the publisher or its search page; the standard text itself is sold by the publisher. Price references are public market ranges, not supplier quotations.